Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178 |
Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | <= 140 MPa | <= 20300 psi | ISO 178 |
Polykemi AB POLYsan FL100 F20 SAN, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 140 MPa | <= 20300 psi | ISO 178 |
Polykemi AB SCANAMID 66 A12^ X30 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 140 - 160 MPa | 20300 - 23200 psi | Injection; ISO 178 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Flexural Strength | <= 140 MPa | <= 20300 psi | ISO 178 |
Polykemi AB POLYfill PPH GF5040 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Strength | 140 - 160 MPa | 20300 - 23200 psi | Injection; ISO 178 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Flexural Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Flexural Strength | 140 MPa | 20300 psi | |
Lehmann & Voss LUVOCOM® 1105-8135/VI PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Flexural Strength | 140 MPa | 20300 psi | |
Manifattura Cattaneo PA 6 G Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
Gromax PBT 4115-104D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Strength | 140 MPa | 20300 psi | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Flexural Strength | 140 MPa | 20300 psi | 5 mm/min; ISO 178 |
Gromax BTG30-DN03N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178-93 |
Wellman Wellamid® MR410 22H-GY1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178 |
Polyplastics Duranex® 701SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM-D790 |
Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber A CHEMICALLY COUPLED 30% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
Flexural Strength | 140 - 160 MPa | 20300 - 23200 psi | At Rupture; ISO 178 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178 |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR BK851 is a 20% glass fiber reinforced flame retardant black polybutylene tere.. |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, Conditioned Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
BLUESTAR 403HF-G20 PBT, 20% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
Aclo Accutech Nylon 6 NY0730G10L Glass Reinforced |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
Beijing Chemical Industry KAIFA® 301-G15 PBT Resin 15% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Strength | >= 140 MPa | >= 20300 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe. |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |
|||
Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
Sumitomo Bakelite North America FM 4008 Fiberglass and Mineral Reinforced Phenolic Resole FM 4008 is a fiberglass and mineral reinforced phenolic resole compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North A.. |
|||
Flexural Strength | 140 MPa | 20300 psi | ISO 178 |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |