Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.55 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
4.78 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.78 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.35 mm |
4.78 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 3.17 mm |
4.78 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 3.17 mm |
4.78 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 3.17 mm |
4.78 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 3.17 mm |
4.78 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.35 mm |
4.78 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chi Mei Polylac® PA-717C ABS Medium impact |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 3.17 mm |
4.78 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.35 mm |
4.78 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chi Mei Polylac® PA-746H ABS - High Flow Super high flow, medium impact |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.78 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.55 J/cm @Thickness 6.35 mm |
4.78 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |