Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 22.8 °C |
15.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 22.8 °C |
15.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Izod Impact, Notched | 8.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 8.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-500-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 8.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM-D256 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM-D256 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj.. |
|||
Izod Impact, Notched | 8.02 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 8.02 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 1012 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 8.00 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Izod Impact, Notched | 8.00 - 9.00 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
15.0 - 16.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NYLON 6615 Black, Super Tough Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 9211 Rigid PVC, Molding Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall HF-6597 Rigid PVC, Molding Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall SP-7107 Rigid PVC, Molding Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it .. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9420 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9420 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies .. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Izod Impact, Notched | 8.00 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-500-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |