Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
1.50 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature -40.0 °C |
1.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature 22.8 °C |
1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PA4/6 HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8007 Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 3.0%); ASTM-D256 |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -40.0 °C |
1.50 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.75%); ASTM-D256 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcementHigh dimensional stability, high stiffnessInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1030 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good impact resistance, high gloss, good light resistance, good processabilityInformation provided by Cos.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP KUR 0550 V0 HF Flame Retardant Polypropylene PP copolymer elastomer modifiedFlame retardant class V0, halogen free, high impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | >= 0.800 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
>= 1.50 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 |
Axiall SP-6655 Rigid PVC, Molding Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall UV-6670 Rigid PVC, Molding Georgia Gulf UV-6670 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -20.0 °C |
1.50 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 6.35 mm |
1.50 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 5006 Rigid PVC, Extrusion, Natural Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf.. |