Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.18 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.50 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.256 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI921NS ASA Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and .. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR490 ABS, Heat Resistance, Low Emission Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.21 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical 60HR HIPS Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.21 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.21 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |