Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
|
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP500N Injection Molding Grade Polypropylene Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen RP344R Injection Molding Grade Polypropylene Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP641P Injection Molding Grade Polypropylene Moplen EP641P is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP641P is a block copolymer suitable for injection molding of c.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.50 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.256 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform.. |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HI5204G PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5204B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HM5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.35 mm |
0.918 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.35 mm |
0.918 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H570P High Density Polyethylene Pipe Resin Key Characteristics: High stiffness, good processingRecommended Applications: Corrugated pipes, non pressure pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 0.000 °C |
0.918 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm |
0.918 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG1130 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |