Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.04 GPa Grade Count:2 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ASTM D638 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ASTM D638 |
Spartech Royalite R61M Low Smoke Resin Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 33LL247 OPP Film Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38LL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38LW280 OPP Film Product Description: A super white opaque slip controlled, biaxially oriented polypropylene film, metalized on one side. Designed for use in reel-fed wrap-around applications, where outstanding meta.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LTL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired. 47LTL247 with supplied .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38ICE M OPP Film Product Description: A coextruded super white opaque, low density, biaxially oriented polypropylene film, metalized on one side. This film is designed for HFFS applications, heat seal or cold seal.A.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38MW280 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38MW480 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features: Outstanding opacity an.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 35MW647 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38ICE OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 47MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Conditioned; ISO 178 |
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene PMD 50213 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 33ICE OPP Film Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 33MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW647 OPP Film Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene H 552 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |