Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 72.0 GPa | >= 10400 ksi | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Piezo Kinetics 406 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars. PKI 406 is suitabl.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Piezo Kinetics 802 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp.. |
|||
Modulus of Elasticity | >= 72.0 GPa | >= 10400 ksi | |
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | Young's Modulus |
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Schott Glass 8516 Sealing Glass Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Schott LITHOSIL-Q Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | tensile |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | tensile |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | tensile |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | tensile |
Constellium Certal® SPC Aluminum Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | tensile |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Modulus of Elasticity | 72.0 GPa | 10400 ksi | tensile |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Modulus of Elasticity | 71.7 GPa | 10400 ksi | |
Corning Large Cover Gorilla® Glass Touch Screen Glass Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C.. |
|||
Modulus of Elasticity | 71.7 GPa | 10400 ksi | |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Modulus of Elasticity | 71.7 GPa | 10400 ksi | Fully Hardened |
ATI Wah Chang Tiadyne™ 3510 Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang |