Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 1.00 GPa | >= 145 ksi | ISO.178 DN.53452 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300 PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom.. |
|||
Modulus of Elasticity | >= 1.00 GPa | >= 145 ksi | ISO.178 DN.53452 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300 PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom.. |
|||
Modulus of Elasticity | 1.00 - 1.20 GPa | 145 - 174 ksi | ASTM D638-04 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 1.00 - 138 GPa | 145 - 20000 ksi | Average value: 22.1 GPa Grade Count:181 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Modulus of Elasticity | 1.00 - 2.65 GPa | 145 - 384 ksi | Average value: 2.09 GPa Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 1.00 - 1.40 GPa @Temperature 60.0 - 120 °C |
145 - 203 ksi @Temperature 140 - 248 °F |
Average value: 1.20 GPa Grade Count:1 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Modulus of Elasticity | 1.00 - 3.10 GPa | 145 - 450 ksi | Average value: 1.86 GPa Grade Count:29 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Modulus of Elasticity | 1.00 - 2.69 GPa | 145 - 390 ksi | Average value: 1.80 GPa Grade Count:22 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | 1 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Modulus of Elasticity | 1.00 - 2.06 GPa | 145 - 298 ksi | Average value: 1.49 GPa Grade Count:6 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 1.00 - 15.0 GPa | 145 - 2180 ksi | Average value: 8.43 GPa Grade Count:471 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 1.00 - 1.50 GPa | 145 - 218 ksi | |
Hybrid Plastics POSS® EP 2000 Epoxy Adhesive EP2000 is a POSS® based, ultra-high temperature epoxy adhesive. The POSS® content in EP2000 offers unique properties such as high thermal stability, outstanding oxygen and chemical resistance... |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | ISO 527 |
GEHR Plastics PA 6 Nylon 6, Conditioned Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | DMA |
Lord Adhesives Circalokâ„¢ EP-729 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-729 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | DMA |
Lord Adhesives Circalokâ„¢ EP-937 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-937 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Modulus of Elasticity | 1.00 GPa @Temperature 20.0 °C |
145 ksi @Temperature 68.0 °F |
|
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | DMA |
Lord Adhesives Circalokâ„¢ EP-939 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-939 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | ISO 178 |
Addiplast Addilene J 310 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | Conditioned; ISO 178 |
Addiplast Addilene J 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 E Flame Retardant Nylon 6 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | DIN EN ISO 527 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Modulus of Elasticity | 1.00 GPa @Temperature 80.0 °C |
145 ksi @Temperature 176 °F |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | ISO 527 |
BASF Ultramid® B3K PA6 (Conditioned) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Modulus of Elasticity | 1.00 - 1.20 GPa | 145 - 174 ksi | |
Biomer P240 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | Conditioned; ISO 178 |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
BASF Ultramid® B3K BK00464 PA6 (Conditioned) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Modulus of Elasticity | 1.00 - 15.0 GPa | 145 - 2180 ksi | Average value: 7.98 GPa Grade Count:413 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Modulus of Elasticity | 1.00 - 5.10 GPa | 145 - 740 ksi | Average value: 1.79 GPa Grade Count:35 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |