Polymer Property : Modulus of Elasticity = 450 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.02 - 3.10 GPa
293 - 450 ksi
Average value: 2.52 GPa Grade Count:36
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 1.86 - 3.10 GPa
270 - 450 ksi
Average value: 2.80 GPa Grade Count:8
Overview of materials for Acrylic, High Flow, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app..
Modulus of Elasticity 1.79 - 3.10 GPa
260 - 450 ksi
Average value: 2.68 GPa Grade Count:16
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 1.00 - 3.10 GPa
145 - 450 ksi
Average value: 1.86 GPa Grade Count:29
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Modulus of Elasticity 2.21 - 3.10 GPa
320 - 450 ksi
Average value: 2.66 GPa Grade Count:24
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled