Hybrid Plastics POSS® EP 2000 Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Hybrid Plastics
Trade Name POSS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hybrid Plastics POSS® EP 2000 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EP2000 is a POSS® based, ultra-high temperature epoxy adhesive. The POSS® content in EP2000 offers unique properties such as high thermal stability, outstanding oxygen and chemical resistance. It provides an exceptional transparent adhesive in these high temperature conditions for metallic, molded plastic and composite materials. Major applications include composites, medical devices, and electronics.Information provided by Hybrid Plastics
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
after cure
Viscosity <= 5000 cP
<= 5000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Modulus of Elasticity 1.00 - 1.50 GPa
145 - 218 ksi
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg >= 300 °C
>= 572 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 6.00 min

@Temperature 80.0 °C
0.100 hour

@Temperature 176 °F
Pot Life 180 min
180 min
Shelf Life 6.00 - 12.0 Month
6.00 - 12.0 Month