| Category | Polymer , Thermoplastic , Polyethylene (PE) |
| Manufacturer | Micropol Limited |
| Trade Name | Isoplas |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Micropol Isoplas P501 Crosslinkable Polyethylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
| Melt Flow | 3.0 g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C |
3.0 g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
| 6.50 MPa <br>@Temperature 100 °C |
943 psi <br>@Temperature 212 °F |
ASTM D638 | |
| Elongation at Break | 200 % | 200 % | |
| Modulus of Elasticity | 1.20 GPa | 174 ksi | 0°C; ASTM D638 |
| 1.00 GPa <br>@Temperature 20.0 °C |
145 ksi <br>@Temperature 68.0 °F |
||
| 1.40 GPa <br>@Temperature -40.0 °C |
203 ksi <br>@Temperature -40.0 °F |
ASTM D638 | |
| Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | BS 2782.306A |
| 1.40 J/cm <br>@Temperature -20.0 °C |
2.62 ft-lb/in <br>@Temperature -4.00 °F |
BS 2782.306A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 90.0 µm/m-°C <br>@Temperature -20.0 °C |
50.0 µin/in-°F <br>@Temperature -4.00 °F |
ASTM D696 |
| 140 µm/m-°C <br>@Temperature 20.0 °C |
77.8 µin/in-°F <br>@Temperature 68.0 °F |
ASTM D696 | |
| 500 µm/m-°C <br>@Temperature 100 °C |
278 µin/in-°F <br>@Temperature 212 °F |
ASTM D696 | |
| Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
| Thermal Conductivity | 0.460 W/m-K | 3.19 BTU-in/hr-ft²-°F | |
| Vicat Softening Point | 124 °C | 255 °F | ASTM D1525 |