Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 300 °C |
19 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 3413R PC 30% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors.
US .. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Asia Pacific) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 190 °C |
19 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Melt Flow | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Melt Flow | 19 g/10 min @Load 3.80 kg, Temperature 230 °C |
19 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 300 °C |
19 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 300 °C |
19 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 300 °C |
19 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 266 °C |
19 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 265 °C |
19 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS 2022 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS 8001A Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 265 °C |
19 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Melt Flow | 19 g/10 min @Load 5.00 kg, Temperature 266 °C |
19 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Melt Flow | 19 g/10 min @Load 2.16 kg, Temperature 265 °C |
19 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-727 ABS Electro-plating |