Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 220 °C
18 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East)
CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona..
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG47 ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG47F ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 260 °C
18 g/10 min

@Load 4.76 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East)
Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 220 °C
18 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East)
Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This ..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® FXM123R PC
FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package ..
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Polimeri Europa SINKRAL G320 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 230 °C
18 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800R PC
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1803R PC
PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was..
Melt Flow 18 - 24 g/10 min

@Load 5.00 kg,
Temperature 230 °C
18 - 24 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF)
Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 265 °C
18 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 266 °C
18 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 200 °C
18 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D1238
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East)
VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 260 °C
18 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics NORYL N850 PPE+PS
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 260 °C
18 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific)
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 250 °C
18 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Melt Flow 18 g/10 min

@Load 21.6 kg,
Temperature 220 °C
18 g/10 min

@Load 47.6 lb,
Temperature 428 °F
ASTM D 1238
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information..
Melt Flow 18 g/10 min

@Load 21.6 kg,
Temperature 190 °C
18 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
This hexene copolymer is tailored for pipe applications that require:Good melt strengthGood pipe stiffnessOutstanding ESCRTypical corrugated pipe applications for HP076 include:Culverts and storm se..
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 230 °C
18 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238 (I)
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Copyright © lookpolymers.com All Rights Reserved