Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 200 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com.. |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene EX2 (HF 7750) is high density polyethylene with propylene as co monomer. It has a medium molar mass with a narrow molar mass distribution.Application: production of monofilaments with high tensile.. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8005 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron Pulse® A20-95 PC/ABS A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren.. |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions .. |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers pigmented red with very low .. |
|||
Melt Flow | 2.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-747R ABS - Extrusion Attach case and refrigerator |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 1502 Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 3501E Natural 1002 ESCR Extrusion Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9901B ABS/PC Blow Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9901B-50148 ABS/PC Blow Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA 91802 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S950 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA TWP 121 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers Diamaloy ABS VP-22 Flame Retardant ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY VP22 Flame Retardant ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Melt Flow | 2.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | <= 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
<= 2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Melt Flow | 2.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 200 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 2.5 g/10 min @Load 3.80 kg, Temperature 190 °C |
2.5 g/10 min @Load 8.38 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Elastamax HTE 2101-1002 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |