Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ABSPC 9901B ABS/PC Blow Molding Grade, High Impact

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ABSPC 9901B ABS/PC Blow Molding Grade, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 2.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
5.2 g/10 min

@Load 5.00 kg,
Temperature 265 °C
5.2 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 50.6 MPa
7340 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.177 GPa
315.7 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 133 °C

@Load 1.00 kg,
Thickness 3.17 mm
271 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Users viewing this material also viewed the following: