BASF Ecovio® C2224 F Blend Biodegradable Polyester

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polylactic Acid (PLA) Biopolymer
Manufacturer BASF
Trade Name Ecovio®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ecovio® C2224 F Blend Biodegradable Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic acid (PLA, NatureWorks®). Because of the PLA content Ecovio® F Blend C2224 consists of 45% of renewable resources. Ecoflex® F Blend is the coherent phase in the structure of Ecovio® F Blend C2224 transferring the beneficial film properties of Ecoflex® F Blend into the new film product.Application: Ecovio® F Blend C2224 has been developed for the conversion to flexible films using a blown film process. Typical applications are packaging films, hygienic films, carrier bags and compost bags. In view of numerous factors influencing functionality and shelf life of Ecovio® films and finished articles made therof the production parameters have to be tested by the converters before utilization. Additionally sufficient field tests are required to ensure the right functionality of the articles made from Ecovio® F Blend C2224.Information provided by BASF
Physical Properties Metric English Comments
Density 1.24 - 1.26 g/cc
0.0448 - 0.0455 lb/in³
ISO 1183
Water Vapor Transmission 98.0 g/m²/day
6.31 g/100 in²/day
ASTM F1249
Oxygen Transmission Rate 860 cc/m²/day
55.4 cc/100 in²/day
dry; ASTM D3985
Melt Flow <= 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
2.4 - 5.2 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.4 - 5.2 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength 27.0 - 35.0 MPa
3920 - 5080 psi
ISO 527
Tensile Strength, Ultimate 27.0 - 35.0 MPa
3920 - 5080 psi
ISO 527
Elongation at Break 250 - 320 %
250 - 320 %
ISO 527
Tensile Modulus 0.520 - 0.750 GPa
75.4 - 109 ksi
ISO 527
Dart Drop Total Energy 380 J/cm
0.712 ft-lb/mil
DIN 53373
Thermal Properties Metric English Comments
Melting Point 110 - 120 °C
230 - 248 °F
DSC
140 - 155 °C
284 - 311 °F
DSC
Vicat Softening Point 68.0 °C
154 °F
A/50; ISO 306
Optical Properties Metric English Comments
Haze 85 %
85 %
ASTM D1003