Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Flex® TPO D-6509 Multi-Flex® A-6509 thermoplastic elastomer blend is designed to provide processors with cost effective compounds with excellent tear strength, tensile strength and high elongation. Multi-Flex® A-.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Sclair® IG454-A Compression Molded HDPE Resin IG454-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG454.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips Sumika Marlex® CHP-035 Thermoplastic Polyolefin
(discontinued **) Applications: Painted air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Melt Flow | 9.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Centrex® 814 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL HI5204G PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 5009 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chase Plastics CP Pryme® AC100-9 Acetal Copolymer Molding Resin Information provided by Chase Plastics. |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 240 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 464 °F |
ISO 1133 |
Polyram RamLloy PBB702 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White 8350 AP Concentrate Based In LDPE DescriptionPOLYBATCH® 8350 AP is an advanced performance white color concentrate containing 50% TiO2 based in LDPE. This product has been specifically engineered to provide improved resistance to .. |
|||
Melt Flow | 9.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1020 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 9.0 - 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 - 13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Cossa Polimeri ESTALENE EN 10 SSC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 9.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
9.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HPA 020 Wire & Cable High Density Polyethylene Resin Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer sh.. |
|||
Melt Flow | 9.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg |
9.0 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow DOWLEX™ IP-10262 High Density Polyethylene DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 TF POM Tribological modified grade low level addition of PTFE, which lower coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 2527 POM Copolymer, 25% glass fiber reinforced POM-GF25Information provided by BARLOG plastics GmbH. |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | ISO 1133 D |
Asahi Kasei Tenac®-C 4563 Copolymer Acetal Resin Weather-Resistant grade containing UV absorber and other additives for superior weathering abilityInformation provided by Asahi Kasei Corporation. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram PM3013G2 Acetal, 10% Glass Fiber
(discontinued **) 10% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melt Flow | 9.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
9.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 9025 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1410MB Polyolefin TPO Granules, Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |