Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | LAB 012 |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 260 °C |
24 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 B |
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | Melt Flow Ratio (I10/I2) is 7.4; ASTM D1238 |
Huntsman Rexell® L2102 Injection Molding LLDPE
(discontinued **) Linear low density copolymer, injection molding, FDA compliant.Features: High flow, medium flex with good environmental stress crack (ESCR), and warpage resistance.Applications: Fitments, large lids.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD500 LDPE
(discontinued **) Features: High Clarity, High Flow, Narrow Molecular Wt. Dist., Good Processability, Warp ResistantUses: Drink LidsApprovals: FDA 21 CFR 177.1520(c) 2.2 and ASTM D 1248, I, Class A, Cat. 1Processing .. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | ISO 1133 |
LATI LATAN 23 Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 24 g/10 min @Load 6.60 kg, Temperature 337 °C |
24 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method). |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 250 °C |
24 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 250 °C |
24 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® CA-7009 PA/PPE, Antistatic Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SK Chemicals SKYPEL M572CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® MB/ML 87 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8350 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8350 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8350 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8350 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
E-Polymers EFLEX® M400 PP Homopolymer M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | ASTM D1238 |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Melt Flow | 24 g/10 min @Load 1.20 kg, Temperature 300 °C |
24 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® Rx1851 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 3375RM Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPAULINS |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | ASTM D1238 |
Huntsman PE2053 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewar.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8350 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8350 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
BP Amoco Acctuf® 3638 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Compounding, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 250 °C |
24 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |