| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 24 g/10 min | 24 g/10 min | LAB 012 |
|
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym..
|
|||
| Melt Flow | 24 - 26 g/10 min | 24 - 26 g/10 min | ASTM D1238 |
|
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 260 °C |
24
g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific)
Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope..
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 260 °C |
24
g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom..
|
|||
| Melt Flow | 24 g/10 min | 24 g/10 min | Melt Flow Ratio (I10/I2) is 7.4; ASTM D1238 |
|
Huntsman Rexell® L2102 Injection Molding LLDPE
(discontinued **)
Linear low density copolymer, injection molding, FDA compliant.Features: High flow, medium flex with good environmental stress crack (ESCR), and warpage resistance.Applications: Fitments, large lids..
|
|||
| Melt Flow |
24
g/10 min @Load 2.16 kg, Temperature 190 °C |
24
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
Yparex 8125 Polyolefin Adhesive Resin
The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer..
|
|||
| Melt Flow | 24 g/10 min | 24 g/10 min | Condition I; ASTM D1238 |
|
Plaskolite Optix® PL-200 Acrylic Resin
(discontinued **)
Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| Melt Flow |
24
g/10 min @Load 2.16 kg, Temperature 190 °C |
24
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade
Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous..
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 200 °C |
24
g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
|
Kraton® D1113 B (SIS) Linear Triblock Copolymer
Description: Kraton D1113 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from South America in the physical form identified: ..
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 300 °C |
24
g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
|
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Melt Flow |
24
g/10 min @Load 6.60 kg, Temperature 337 °C |
24
g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
|
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
|
|||
| Melt Flow |
24
g/10 min @Load 6.60 kg, Temperature 337 °C |
24
g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
|
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method).
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 250 °C |
24
g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| Melt Flow |
24
g/10 min @Load 10.0 kg, Temperature 250 °C |
24
g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
|
Samsung Cheil Industries Infino® LS-1150G PC/ABS, 15% Glass Filled FR
15% GF reinforcement; can be used in mold frames for LCD BLU.Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 300 °C |
24
g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
|
Samsung Cheil Industries Infino® CA-7009 PA/PPE, Antistatic
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
24
g/10 min @Load 5.00 kg, Temperature 260 °C |
24
g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
|
Styron Pulse® 2000EZ PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Melt Flow |
24
g/10 min @Load 6.60 kg, Temperature 337 °C |
24
g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
|
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing.
|
|||
| Melt Flow |
24
g/10 min @Load 10.00 kg |
24
g/10 min @Load 22.05 lb |
ASTM D1238 |
|
Sumitomo Chemical ESPOLEX® 4855 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Melt Flow |
24
g/10 min @Load 2.16 kg, Temperature 230 °C |
24
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
SK Chemicals SKYPEL P137DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
|
|||
| Melt Flow |
24
g/10 min @Load 2.16 kg, Temperature 230 °C |
24
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Carmel Olefins CAPILENE® T 12 EV Polypropylene Homopolymer
CAPILENE® T 12 EV is a polypropylene homopolymer with narrow molecular weight distribution, controlled rheology, intended for fiber applications. It is characterized by easy processing, very good m..
|
|||
| Melt Flow | 24 - 36 g/10 min | 24 - 36 g/10 min | |
|
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
|
|||
| Melt Flow | 24 - 36 g/10 min | 24 - 36 g/10 min | |
|
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
|
|||
| Melt Flow | 24 g/10 min | 24 g/10 min | Melt Flow Ratio (I10/I2) is 7.3; ASTM D1238 |
|
Huntsman Rexell® L2101 Injection Molding LLDPE
(discontinued **)
Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,..
|
|||
| Melt Flow |
24
g/10 min @Load 1.20 kg, Temperature 275 °C |
24
g/10 min @Load 2.65 lb, Temperature 527 °F |
DAM; cm³/10min; ISO 1133 |
|
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
|
|||
| Melt Flow |
24
g/10 min @Load 2.16 kg, Temperature 230 °C |
24
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
IRPC Polimaxx Polene 3375RM Polypropylene Random Copolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPAULINS
|
|||
| Melt Flow | 24 g/10 min | 24 g/10 min | ASTM D1238 |
|
Huntsman PE2053 Injection Molding Polyethylene
(discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewar..
|
|||