M. Holland Company LD500 LDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company LD500 LDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: High Clarity, High Flow, Narrow Molecular Wt. Dist., Good Processability, Warp ResistantUses: Drink LidsApprovals: FDA 21 CFR 177.1520(c) 2.2 and ASTM D 1248, I, Class A, Cat. 1Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 0.248 GPa
36.0 ksi
1% Secant; ASTM D790
0.262 GPa
38.0 ksi
3% Tangent; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature -38.0 °C
-36.4 °F
ASTM D746
Descriptive Properties Value Comments
Form Pellets