Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Pro® 5012 C Natural Polypropylene Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom PLASTAMID® 6 BT N 29 B PA6 Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivered in the natu.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Ineos ABS Lustran® 2863
(discontinued **) Special grade for smart cards.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 2564PCX TA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTH CONTAIN UV STABILIZER AND LONG TERM HEAT AGING ADDITIVESAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, .. |
|||
Melt Flow | 13 g/10 min | 13 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® J-61/10 Polypropylene Copolymer, 10% Glass Fiber Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 13 g/10 min | 13 g/10 min | ASTM D 1238 |
MRC Polymers NAXALOY™ 793MF6 PC + Polyester Blend, 6% Mineral Filled • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Flow | 13 g/10 min @Load 6.60 kg, Temperature 337 °C |
13 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Melt Flow | 13 - 15.9 g/10 min | 13 - 15.9 g/10 min | |
Shuman 881 Grey Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 240 °C |
13 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Styrolution Terblend® N NM-13 ABS/PA6 (Dry) Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by .. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SK Chemicals SKYPEL G168D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyram RamOfin PPH316G4 Polypropylene, 20% Glass Fiber 20% Glass fiber reinforced, high heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
13 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE109AE TPO Compound Daplen EE109AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE109AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
13 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSI 625 Polystyrene Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi.. |
|||
Melt Flow | 13 g/10 min @Load 8.70 kg, Temperature 190 °C |
13 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® AG2677 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transparent colors on.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil Exxtral™ HMU 404 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, characterized by very high stiffness and high heat stabilization. Typically used in automotive heating and air conditi.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |