Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers NAXALOYâ„¢ 793MF6 PC + Polyester Blend, 6% Mineral Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP
Manufacturer MRC Polymers
Trade Name NAXALOY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers NAXALOYâ„¢ 793MF6 PC + Polyester Blend, 6% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D 792
Water Absorption at Saturation 0.20 - 0.30 %
0.20 - 0.30 %
ASTM D 1238
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D 955
Melt Flow 13 g/10 min
13 g/10 min
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D 638
Elongation at Break 70 %
70 %
ASTM D 638
Flexural Strength 90.0 MPa
13100 psi
ASTM D 790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D 790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D 648