| Category | Polymer , Thermoplastic , Polypropylene (PP) | 
| Manufacturer | Multibase | 
| Trade Name | Multi-Pro® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Multibase Multi-Pro® 5012 C Natural Polypropylene.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 | 
| Linear Mold Shrinkage | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ASTM D955 | 
| Melt Flow |           13           g/10 min           @Load 2.16 kg, Temperature 230 °C  | 
                  13           g/10 min           @Load 4.76 lb, Temperature 446 °F  | 
        ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Ultimate | 13.8 MPa | 2000 psi | ASTM D638 | 
| Elongation at Break | 170 % | 170 % | ASTM D638 | 
| Flexural Strength | 25.9 MPa | 3750 psi | ASTM D790 | 
| Flexural Modulus | 1.72 GPa | 250 ksi | Method I (3 point load), Procedure B); ASTM D790 | 
| Izod Impact, Notched | 2.30 J/cm | 4.30 ft-lb/in | 73°F; ASTM D256 | 
| Gardner Impact | 18.08 J | 13.33 ft-lb | ASTM D3029 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 120 °C | 248 °F | Unannealed; ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | Unannealed; ASTM D648 |