Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Melt Flow | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Flow | 1.2 - 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 - 1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 8300G (EPYS30RE) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem PB 601 LDPE Blow Molding Polyethylene
(discontinued **) Applications: Toys; shrink films for pallets; general purpose; pipes and hoses; serum flasks. Information provided by Braskem |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR .. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238G |
Hannam Chemical Hanalac 770 ABS, Extrusion Grade FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, n.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 7011 TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ISO 1133 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Shuman 790 Black and Custom Colors ABS-Flame Retardant Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Shuman 791 Black and Custom Colors ABS-Flame Retardant Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Melt Flow | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BB213CF Polypropylene Copolymer BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg |
1.2 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Melt Flow | 1.2 g/10 min @Temperature 230 °C |
1.2 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 5100H Extrusion processing Polypropylene HomopolymerApplications: Various extrusion profile, sheet and film applications.Formolene 5100H DEVELOPMENTAL is a high molecular weight, highly isotactic polypropylene homopolymer designed for vari.. |
|||
Melt Flow | 1.2 g/10 min @Temperature 230 °C |
1.2 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t.. |
|||
Melt Flow | 1.2 g/10 min @Load 8.70 kg, Temperature 224 °C |
1.2 g/10 min @Load 19.2 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips Marlex® C100 Polyethylene; Enhanced Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typi.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg |
1.2 g/10 min @Load 4.76 lb |
|
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® LE 6010 HV Nylon Alloy, 10% Glass Fiber Reinforced (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents). 10% glass fiber reinforced. Suited to blow molding of technical pa.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS802L High Impact Grade |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem PH 0130 HOMO Polypropylene Homopolymer PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/im.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |