Material Notes:
HomopolymerApplications: Various extrusion profile, sheet and film applications.Formolene 5100H DEVELOPMENTAL is a high molecular weight, highly isotactic polypropylene homopolymer designed for various extrusion profile, sheet and film applications. It contains a unique combination of stabilizers, which give it process stability and superior end use performance. It does not contain slip or antiblock.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.2 g/10 min

@Temperature 230 °C
1.2 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 10 %
10 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256