Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 7007 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 0.50 g/10 min @Load 0.325 kg, Temperature 270 °C |
0.50 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PC 19 GF 20 PP, 20% glass fibre, mod. of mech. properties FeaturesModified copolymer PP for iextrusion, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied i.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 30-005W Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Antiblock, High Slip, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or .. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips 7105T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | Condition E; ASTM D1238 |
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Flow | 0.50 - 5.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.50 - 5.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | Condition E; ASTM D 1238 |
Eastman 5284 LDPE 8% EVA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, No Slip, High Antiblock, High Coefficient of FrictionApplications:Ice Ba.. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | 2.16 kg at 230C; ASTM D1238 |
Ineos N00GX11 Polypropylene Impact Copolymer Grade N00Gx11 is a fractional melt flow rate experimental impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared .. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 230 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos N00G-01 Polypropylene Impact Copolymer Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 5703 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hostacomâ„¢ CA270G Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CA270G fractional melt flow, 140 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of grain retention characte.. |
|||
Melt Flow | 0.50 - 1.5 g/10 min @Temperature 230 °C |
0.50 - 1.5 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 892E Extrusion and Blow Molding Grade Homopolymer Polypropylene DescriptionPolyfort® FPP 892E is an extrusion and blow molding grade 20% mineral-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Westlake Mxsten CV77519 Polyethylene Plastomer Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin .. |
|||
Melt Flow | 0.50 g/10 min @Temperature 230 °C |
0.50 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 5100J Blown and Cast Film Polypropylene HomopolymerApplications: Cast and blown film applications.Formolene 5100J is a high molecular weight, highly isotactic polypropylene homopolymer designed for sheet, cast and blown film applications... |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Unipetrol PP MONSTEN® EH 001 Polypropylene Homopolymer Applications include extrusions and tapes. LTHA stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.50 - 1.5 g/10 min | 0.50 - 1.5 g/10 min | ISO 1133 |
Chengdu Polyster H4543B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ b.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | ASTM D1238 |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | Melt Flow Ratio = 7.6 (I<sub>10</sub>/I<sub>2</sub>); ASTM D1238 |
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be ut.. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | ASTM D1238 |
Aclo Accutech ABS ABS831G40L Glass Reinforced |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Bapolene® PP5010 Polypropylene, Extrusion Grade Bapolene PP5010 is an extrusion PP high impact copolymer with excellent color and processability. It offers extra high impact strength and low temperature properties.Applications: Auto, pipe, profi.. |
|||
Melt Flow | 0.50 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.50 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Arkema Group Solarkote® P-611 Acrylic PVC capstock, white, low glossInformation provided by Arkema Group |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
E-Polymers EFLEX® S5040 Extrusion S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
E-Polymers EFLEX® S5050 Extrusion S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas.. |
|||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Antiblock, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238/E |
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 235 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® P 60AD Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |