Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos N00GX11 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ineos N00GX11 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade N00Gx11 is a fractional melt flow rate experimental impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impact copolymers. For applications requiring good medium term heat aging performance, Ineos recommends the N00M-00 grade.
Physical Properties Metric English Comments
Melt Flow 0.50 g/10 min
0.50 g/10 min
2.16 kg at 230C; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
at 23C; ASTM D638
Flexural Modulus 1.242 GPa
180.1 ksi
at 23C; ADST D790A
Izod Impact, Notched NB
NB
1/8” (3 mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Descriptive Properties Value Comments
Process Blow Molding
Pipe Extrusion
Sheet Extrusion