Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Orgalloy® P 60AD Nylon (Conditioned)

Category Polymer , Thermoplastic , Nylon
Manufacturer Arkema
Trade Name Orgalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orgalloy® P 60AD Nylon (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 235 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V