Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.6 g/10 min | 2.6 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE D 5302 NAT The moisture content is 0.912%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 2.6 g/10 min | 2.6 g/10 min | ASTM D1238 |
Plaskolite Optix® CA-82 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for injection molding and contains a mold release agent. This resin offers high heat .. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-.. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total 819E Polystyrene
(discontinued **) Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof.. |
|||
Melt Flow | 2.6 g/10 min @Load 1.00 kg, Temperature 235 °C |
2.6 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv.. |
|||
Melt Flow | 2.6 g/10 min @Load 1.00 kg, Temperature 235 °C |
2.6 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Melt Flow | 2.6 - 3.2 g/10 min | 2.6 - 3.2 g/10 min | ±10% |
Kazanorgsintez 276-288 High Density Polyethylene Composite Production Method: Compositions are achieved by gaseous-phase method. Application: Composition is intended for production of polymer film fibers contacting bulk food.Information Provided by Kaza.. |
|||
Melt Flow | 2.6 g/10 min | 2.6 g/10 min | ASTM D1238 |
Hyosung Topilene F400 PP F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Global 120-PC-Natural Acrylonitrile Styrene, General Purpose Grade Description-transparent, natural, medium impact resistance, high hardness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInformation provide.. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global) Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig.. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.6 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.6 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnumâ„¢ PG914 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 260 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 8140 Ionomer Resin, Sodium Surlyn® 8140 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melt Flow | 2.6 g/10 min | 2.6 g/10 min | ASTM D1238 |
Dow 608A Low Density Polyethylene (LDPE) A formulated clarity film resin for thin gauge optical packaging Optimum gauge range: 0.8 - 2.5 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem FF026M Homopolymer Polypropylene Description: Excellent Color and Processing Stability, Superior Optical and Mechanical Properties, Broad Processing WindowApplications: Suggested Uses Include BOPP ApplicationsThis resin meets the r.. |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Arkema Group Kynar® 6000 HDC N 119 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie.. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® PE3507-2 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® PE3507-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applic.. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 510 Bioriented Film Polypropylene Applications: Bioriented films for conversion; adhesive tapes; textile and food packing. Information provided by Braskem |