Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 925A PC Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Melt Flow | 13 g/10 min | 13 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
13 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1170 B (SIBS) Linear Triblock Copolymer Description: Kraton D1165 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: .. |
|||
Melt Flow | 13 g/10 min | 13 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® Elite HH 1827 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hostacomâ„¢ BG722AC Polypropylene Copolymer Description: Hostacomâ„¢ BG722AC medium high melt flow, 1,700 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer is designed with an excellent balance of stiffness, impact r.. |
|||
Melt Flow | 13 g/10 min @Load 6.60 kg, Temperature 337 °C |
13 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg |
13 g/10 min @Load 4.76 lb |
ISO 1133 |
SIDPEC EGYPTENE® HD 5813 EA HDPE Injection Molding Applications:CrateAerosol capsHouse waresInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Valox® V3500EX PBT PBT, Flame Retardant, Heat Stabilized, Extrusion grade for monofilament/Fiber ApplicationThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2795 PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1, 85 oC |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyram RamOfin PPH316G4 Polypropylene, 20% Glass Fiber 20% Glass fiber reinforced, high heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram RamTal PM8515 Acetal, High impact High impact polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Melt Flow | 13 g/10 min | 13 g/10 min | ISO 1133 |
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
Melt Flow | 13 g/10 min | 13 g/10 min | ASTM D1238 |
Tipco Tipcolene® MD-TPE MD TPE - Impact Modified Polypropylene Copolymer Compound for Automobile Bumpers High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® CM600-V TPC-ES FR Extrusion, Flame Retardant (Halogen free) |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 200 °C |
13 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram RamTal PM1113 Polyacetal Copolymer for Injection Molding General purpose polyacetal copolymer for injection molding applications, MFI 13.Information provided by Polyram. |