Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 13 g/10 min

@Load 10.0 kg,
Temperature 220 °C
13 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 51.0 MPa
7400 psi
5 mm/min; ASTM D638
Flexural Strength 73.5 MPa
10700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
B/50; ISO R306
Optical Properties Metric English Comments
Gloss 90 %

@Temperature 23.0 °C
90 %

@Temperature 73.4 °F
50% RH, 60°; ASTM D2457
Descriptive Properties Value Comments
Pencil Hardness H
500g, JIS K 5401