Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Melt Flow | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | Condition E; ASTM D 1238 |
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem PB 601 LDPE Blow Molding Polyethylene
(discontinued **) Applications: Toys; shrink films for pallets; general purpose; pipes and hoses; serum flasks. Information provided by Braskem |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an.. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ HCA155MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115MP is a lubricated and nucleated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21.. |
|||
Melt Flow | 1.2 g/10 min @Load 1.00 kg, Temperature 235 °C |
1.2 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
LyondellBasell Alathon® M4612 High Density Polyethylene ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238G |
Hannam Chemical Hanalac 770 ABS, Extrusion Grade FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, n.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Astryn CA743GA Polypropylene Copolymer Key Features: low melt flow, low modulus, UV-stabilized polypropylene copolymer with antiblock, good heat seamability, good puncture resistance, plasticizer-free, excellent low temperature impact re.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
Shuman 791 Black and Custom Colors ABS-Flame Retardant Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.20 kg |
1.2 g/10 min @Load 4.86 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® 821 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |
|||
Melt Flow | 1.2 g/10 min @Temperature 230 °C |
1.2 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t.. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 1.2 g/10 min @Load 8.70 kg, Temperature 224 °C |
1.2 g/10 min @Load 19.2 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Melt Flow | 1.2 g/10 min | 1.2 g/10 min | ExxonMobil Method |
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® LE 60LM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem PH 0130 HOMO Polypropylene Homopolymer PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/im.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 880 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 880 is an ethylene-vinyl acetate copolymer resin containing slip and anti-block additives for use in industrial applications.Applications: Elvax® 880 resins can be used for the fo.. |