ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications

Category Polymer , Film , Thermoplastic , Elastomer, TPE
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blown film applications requiring outstanding sealability and toughnessAvailability: Latin America, North America and South America Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesApplications:Blown Film Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Thickness 31.8 microns
1.25 mil
Melt Flow 1.2 g/10 min
1.2 g/10 min
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 4.96 MPa
720 psi
ASTM D882
Film Tensile Strength at Yield, TD 4.55 MPa
660 psi
ASTM D882
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 630 %
630 %
ASTM D882
Film Elongation at Yield, MD 9.4 %
9.4 %
ASTM D882
Film Elongation at Yield, TD 8.4 %
8.4 %
ASTM D882
Puncture Energy 7.74 J
5.71 ft-lb
ExxonMobil Method
Elmendorf Tear Strength, MD 5.35 g/micron
136 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 8.82 g/micron
224 g/mil
ASTM D1922
Dart Drop 41.89 g/micron
1064 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 73.50 MPa
10660 psi
ASTM D882
Film Tensile Strength at Break, TD 73.84 MPa
10710 psi
ASTM D882
1% Secant Modulus, MD 73.1 MPa
10600 psi
ASTM D882
1% Secant Modulus, TD 77.2 MPa
11200 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 95.6 °C
204 °F
Peak Melting Temperature; ExxonMobil Method
Crystallization Temperature 79.0 °C
174 °F
ExxonMobil Method
Vicat Softening Point 87.8 °C
190 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 2.5 %
2.5 %
ASTM D1003
Gloss 80 %
80 %
ASTM D2457
Descriptive Properties Value Comments
Puncture Force 17 lbf
ExxonMobil Method