Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin Film Properties.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 59A HDPE Injection Molding Resin Features: Homopolymer, high drop impact resistance and high stiffness.Applications: Juice, water containers, personal protective equipment, grain elevator buckets, designed for accumulator and recip.. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion, food and liquid packaging.Data provided by the manufacturer.. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur.. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Sclair® 99K Homopolymer HDPE Film Resin 99K complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Melt Flow | 0.72 g/10 min | 0.72 g/10 min | ASTM D 1238 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufacturer. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |
|||
Melt Flow | 0.72 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 14J1 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, high strength and toughness.Applications: Produce film.Data provided by the manufacturer. |