Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 19MB440 OPP Film Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MB080 OPP Film Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MB400 OPP Film Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MB666 OPP Film Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MB668 OPP Film Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 21MB621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 21MBT621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel.. |
|||
Water Vapor Transmission | 1.40 g/m²/day @Temperature 23.0 °C |
0.0900 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 20MBT666 OPP Film Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as.. |