Physical Properties Metric English Comments
Viscosity 30000 cP
30000 cP
Mixed; TM R050-12
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Viscosity 30000 - 50000 cP
30000 - 50000 cP
Huntsman Araldite PY 307-1 Epoxy Phenol Novolac
Weight per Epoxide (EEW, g/eq) 170 to 179. Max color is 4.Comments/Applications: Epoxy functionality of 2.4. EPN 1139 or EPN 1179 type with much lower viscosity. FDA listed. For high performance..
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive
LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po..
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Viscosity 30000 cP
30000 cP
Before Curing
Silikony Polskie Gumosil WW Silicone Rubber
Flexible with good tearing resistance
Viscosity 30000 - 65000 cP
30000 - 65000 cP
mixed compound; thixotropic
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy
Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun..
Viscosity 30000 - 70000 cP
30000 - 70000 cP
Part A
Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures
Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excel..
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive
TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid..
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Mixed
Trelleborg Emerson & Cuming Stycast® 2741LV/15LV Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
Viscosity 30000 - 40000 cP

@Temperature 23.0 °C
30000 - 40000 cP

@Temperature 73.4 °F
Master Bond Supreme 11 High Peel and Shear Strength Epoxy Adhesive
Master Bond Polymer System Supreme 11 features a unique balance of performance properties including both high shear and high peel strengths. This two component adhesive system is formulated to cure ..
Viscosity 30000 - 40000 cP

@Temperature 23.0 °C
30000 - 40000 cP

@Temperature 73.4 °F
Master Bond UV10TK Dimensionally Stable One Component UV Curable Adhesive
Master Bond UV10TK is a moderate viscosity, one part UV system for bonding, sealing and coating featuring very good optical clarity and excellent physical properties as well as superior temperature ..
Viscosity 30000 cP
30000 cP
Dynamic
Dow Corning 7-3101 Elastomer Blend Hip Emulsion
A concentrated emulsion of dimethicone crosspolymer in cyclopentasiloxane and dimethicone that is designed to facilitate the rapid development of skin care formulations which contain these emollient..
Viscosity 30000 cP
30000 cP
Dynamic
Dow Corning 7-3118 EBAP Hip Emulsion
A concentrated emulsion of dimethicone crosspolymer in cyclopentasiloxane and dimethicone that is designed to facilitate the rapid development of skin care formulations which contain these emollient..
Viscosity 30000 - 80000 cP
30000 - 80000 cP
dynamic
Dow Corning Q2-7735 ADHESIVE
Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning
Viscosity 30000 cP

@Temperature 190 °C
30000 cP

@Temperature 374 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1533E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 30000 cP
30000 cP
Epoxyset Epoxiohm EO-21 Electrically Conductive Epoxy Adhesive
EO-21 is a two part, silver filled high electrical conductivity epoxy adhesive. It is designed to cure at room temperature or rapidly at elevated temperature and exhibits very excellent adhesion and..
Viscosity 30000 - 35000 cP
30000 - 35000 cP
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive
EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl..
Viscosity 30000 cP
30000 cP
Dymax 3073 Solvent-Free Plastic Adhesive
Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide ..
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Abatron AboCast/AboCure 8501-5/8501-4 High Temperature Resistant Epoxy
Gray, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be us..
Viscosity 30000 cP
30000 cP
ACC MM922 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Viscosity 30000 cP
30000 cP
catalyzed with QM CAT PURPLE
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
Viscosity 30000 cP
30000 cP
catalyzed with QM CAT RED 3
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
Viscosity 30000 cP
30000 cP
catalyzed with QM CAT BLUE
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
Viscosity 30000 cP
30000 cP
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Viscosity 30000 cP
30000 cP
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Viscosity 30000 - 70000 cP
30000 - 70000 cP
Accelerator
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Viscosity 30000 cP
30000 cP
Mixed; TM R050-12
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive
Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m..
Viscosity 30000 - 100000 cP
30000 - 100000 cP
Thixotropic
Loctite® 574 Semi-rigid Cure Anaerobic Sealant
Anaerobic GasketingLoctite® 574 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Fast curing, large gaps
Viscosity 30000 cP
30000 cP
Mixed; TM R050-12
Resinlab® EP1305LV Clear Epoxy Casting Resin
Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..