Trelleborg Emerson & Cuming Stycast® 2741LV/15LV Two-Component Easy Mix Ratio Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 2741LV/15LV Two-Component Easy Mix Ratio Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, thermal and mechanical shock resistance, and thermal conductivity.Emerson & Cuming 2741LV/15LV Stycast® Two-Component Easy Mix Ratio EncapsulantMix Ratio by weight = 400:100Good Chemical Resistance Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
Dielectric Strength 15.7 kV/mm
400 kV/in