Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG38U ABS High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC K5025 PP, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5015 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5015 PD1 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF5030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYform POM C M90 GF30 Polyoxymethylene Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ PFA X 6505 UHP Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low levels of metal and .. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 115-1652 LMDPE Rotational Molding Resin Description: ICORENE 115-1652 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Kuraray HYBRAR® Low Rebound Compound # 2 Control Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Kuraray SEPTON® H5127 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Melt Index of Compound | 5.0 - 10 g/10 min | 5.0 - 10 g/10 min | |
Sibur 21080-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 300 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Melt Index of Compound | 5.0 g/10 min @Load 1.20 kg, Temperature 280 °C |
5.0 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Melt Index of Compound | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Melt Index of Compound | 5.0 - 8.0 g/10 min | 5.0 - 8.0 g/10 min | ASTM D1238 |
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow DS6D81 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW DS6D81 Polypropylene Resin is intended .. |
|||
Melt Index of Compound | 5.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 018/27F Halogen Free PVC Sheathing, designed to meet VDE 0207 part 24 HM4 |
|||
Melt Index of Compound | 5.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 018/33 Halogen Free PVC Sheathing, high flexibility |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC GF5020 PB Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH TS5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 5.0 g/10 min | 5.0 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP812 Linear, Medium-Density Polyethylene DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman. |