Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler |
Manufacturer | Polykemi AB |
Trade Name | POLYfill |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Polykemi AB POLYfill PPH GF5015 PD1 PP, Glass Fiber-Reinforced, Chemically Coupled.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
Filler Content | 15 % | 15 % | ±2%; Polykemi |
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | With Flow; ISO 2577 |
0.0080 cm/cm | 0.0080 in/in | Across Flow; ISO 2577 | |
Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | <= 60.0 MPa | <= 8700 psi | ISO/R527 |
Elongation at Break | 5.0 % | 5.0 % | ISO/R527 |
Flexural Strength | <= 90.0 MPa | <= 13100 psi | ISO 178 |
Flexural Modulus | 3.30 GPa @Temperature 23.0 °C |
479 ksi @Temperature 73.4 °F |
ISO 178 |
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | 120°C/h; ISO 75/1 |
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 244 °F | 120°C/h; ISO 75/1 |
Vicat Softening Point | 110 °C @Load 5.001 kg |
230 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
Back Pressure | 1.00 - 2.00 MPa | 145 - 290 psi |
Descriptive Properties | Value | Comments |
---|---|---|
Holding Pressure () | 20-40 | % of injection pressure |
Injection Speed () | High |