| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | Polykemi AB |
| Trade Name | POLYfill |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYfill PPC K5025 PP, Mineral Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
| Filler Content | 25 % | 25 % | ±2%; Polykemi |
| Melt Index of Compound | 5.0 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
5.0 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 20.0 MPa | <= 2900 psi | ISO/R527 |
| Elongation at Yield | 7.0 % | 7.0 % | ISO/R527 |
| Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
| Flexural Modulus | 1.60 GPa <br>@Temperature 23.0 °C |
232 ksi <br>@Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.500 J/cm² <br>@Temperature 23.0 °C |
2.38 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 70.0 °C <br>@Load 5.001 kg |
158 °F <br>@Load 11.03 lb |
50°C/h; ISO 306 |
| 135 °C <br>@Load 1.00 kg |
275 °F <br>@Load 2.21 lb |
50°C/h; ISO 306 | |
| Flammability, UL94 | HB <br>@Thickness 1.60 mm |
HB <br>@Thickness 0.0630 in |
|
| Glow Wire Test | 750 °C <br>@Thickness 2.00 mm |
1380 °F <br>@Thickness 0.0787 in |