| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
| Filler Content | 30 % | 30 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | With Flow; ISO 2577 |
| 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 72.0 MPa | <= 10400 psi | ISO/R527 |
| Elongation at Yield | 8.0 % | 8.0 % | ISO/R527 |
| Flexural Strength | <= 122 MPa | <= 17700 psi | ISO 178 |
| Flexural Modulus | 7.50 GPa @Temperature 23.0 °C |
1090 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 165 °C | 329 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 160 °C @Load 5.001 kg |
320 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| 168 °C @Load 1.00 kg |
334 °F @Load 2.21 lb |
50°C/h; ISO 306 | |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
| Glow Wire Test | 550 °C @Thickness 1.60 mm |
1020 °F @Thickness 0.0630 in |
IEC 695-2-1 |