Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 85FS PC/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 85FS UV PC/ABS-Blend, UV stabilized Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC TS25020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 g/10 min @Load 4.76 lb, Temperature 482 °F |
±5; cm³/10min; ISO 1133 |
PolyOne Bergadur™ PB40 G15 blue Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Melt Index of Compound | 25 g/10 min | 25 g/10 min | |
Sibur PL-1GS Polyvinyl Chloride (PVC) For the production of boot tops and soles of autumn-spring purpose and for production of boots by molding method under pressure. |
|||
Melt Index of Compound | 25 - 31 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 - 31 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Melt Index of Compound | 25 - 31 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 - 31 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East) high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop.. |
|||
Melt Index of Compound | 25 - 35 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 - 35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |
|||
Melt Index of Compound | 25 g/10 min | 25 g/10 min | ASTM D1238 |
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |