Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0040 - 0.0080 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0050 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0040 - 0.0080 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0040 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0050 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.0394 in |
DAM |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0060 - 0.0080 in/in @Thickness 0.0394 in |
|
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm @Thickness 3.17 mm |
0.0040 - 0.0080 in/in @Thickness 0.125 in |
Direction of Flow; ASTM D955 |
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm @Thickness 3.17 mm |
0.0040 - 0.0080 in/in @Thickness 0.125 in |
Transverse to Flow; ASTM D955 |
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0050 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |