Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 1.60 mm |
0.010 in/in @Thickness 0.0630 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 1.60 mm |
0.010 in/in @Thickness 0.0630 in |
Flow; DAM |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 1.60 mm |
0.010 in/in @Thickness 0.0630 in |
Transverse; DAM |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
DAM |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm @Thickness 3.17 mm |
0.010 - 0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/20/FD Polypropylene Homopolymer, 20% Talc Filled, FDA compliant Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm @Thickness 3.00 mm |
0.010 - 0.013 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm @Thickness 3.00 mm |
0.010 - 0.013 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 1.60 mm |
0.010 in/in @Thickness 0.0630 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm @Thickness 1.60 mm |
0.010 - 0.016 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |