Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm @Thickness 3.17 mm |
0.0080 - 0.012 in/in @Thickness 0.125 in |
|
Ovation Polymers OPTRENE 20GF Polypropylene, 20% Glass Reinforced Properties of chemically coupled glass reinforced (20%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | |
LATI Laticonther 47/1 CP/80 PP Copolymer High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Latistat 83-05 POM, Impact Modified Dissipative product based on Polyamide 12 (PA12), impact modified. Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF00469S PA 66 LNP* THERMOCOMP* RF00469S is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF00469S PA 66 (Asia Pacific) LNP* Thermocomp* RF00469S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA 30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | Borealis Method |
Borealis Xmod™ GB305HP High Performance 35% Glass Fiber Reinforced Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GF30-60 XE-WBK Nylon 6, 30% Glass Reinforced, Weatherable All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT13-66 XE-NBK1 13% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GFT33N051-NBK2 Nylon 66, 33% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6 Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® MR409 22H-NBK4 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-GY1 40% Mineral/Glass Fiber Reinforced Nylon 6 Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ISO 294 |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latilub 66-15ST G/30 PA66, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |