Polymer Property : Linear Mold Shrinkage, Transverse = 0.0035 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific)
Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Linear Mold Shrinkage, Transverse 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
Test Condition: 150x105x3; acc. ISO 2577
Ineos ABS Lustran® SAN GF20 Glass Fiber Reinforced
Linear Mold Shrinkage, Transverse 0.0020 - 0.0035 cm/cm
0.0020 - 0.0035 in/in
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa..
Linear Mold Shrinkage, Transverse 0.0020 - 0.0035 cm/cm
0.0020 - 0.0035 in/in
Test Condition: 150x105x3; acc. ISO 2577
Ineos ABS Lustran® SAN GF30 Glass Fiber Reinforced
Linear Mold Shrinkage, Transverse 0.0020 - 0.0035 cm/cm
0.0020 - 0.0035 in/in
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC
LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+PS
LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS
LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced, flame retardant material.
Linear Mold Shrinkage, Transverse 0.0015 - 0.0035 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0035 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.