Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)  (Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
LATI
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
Test Condition: 150x105x3; acc. ISO 2577
Ineos ABS Lustran® SAN GF20 Glass Fiber Reinforced
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
ISO 2577
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
ISO 2577
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0040 cm/cm
0.0025 - 0.0040 in/in
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0055 cm/cm
0.0025 - 0.0055 in/in
LATI Laticonther 82 CP1/800 PA12
High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0040 cm/cm
0.0025 - 0.0040 in/in
LATI Latilub 87/28-15T K/20 PC, 20% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0045 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0045 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
Linear Mold Shrinkage, Transverse 0.0025 - 0.0040 cm/cm

@Time 86400 sec
0.0025 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp GC006XXZ PSU
LNP THERMOCOMP* GC006XXZ is a compound based on Polysulfone resin containing Carbon Fiber.This product is also known as Thermocomp* GC-1006.This data was supplied by SABIC-IP for the Americas region..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0076 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0076 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP
30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited).
Linear Mold Shrinkage, Transverse 0.0025 - 0.0076 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0076 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Asia Pacific)
30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited).
Linear Mold Shrinkage, Transverse 0.0025 cm/cm

@Thickness 6.40 mm
0.0025 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Linear Mold Shrinkage, Transverse 0.0025 cm/cm

@Thickness 6.40 mm
0.0025 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0045 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL EM7304F PPE+PS
15% glass reinforced, high flow with enhanced polyurethane foam adhesion for instrument panel retainers.
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications.
Linear Mold Shrinkage, Transverse 0.0025 cm/cm
0.0025 in/in
LATI
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)  (discontinued **)
Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0065 cm/cm
0.0025 - 0.0065 in/in
LATI Latigea B01 I6 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...