Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant Halogen and phosphor freeInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armlen® PP MF 40-4M Polypropylene Copolymer, 40% Calcium Carbonate High impact resistance at low temperatureInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Transverse | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | |
LATI Laticonther 47/1 CP/80 PP Copolymer High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latimass 75/4-04 D009 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latiohm 82-02 PD09 PA12 Semiconductive/dissipative product based on Polyamide 12 (PA12). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
LATI Latiohm 83-07 PD11 CNT PA12, Impact Modified Semiconductive/dissipative product based on Polyamide 12 (PA12), impact modified. Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 (Asia Pacific) LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm @Time 86400 sec |
0.0080 - 0.012 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched (Europe-Africa-Middle East) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | Borealis Method |
Borealis Xmod™ GB305HP High Performance 35% Glass Fiber Reinforced Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman EcoLon® 2200-BK1 Nylon 66, 40% Mineral/Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GF1864-WBK1 Nylon 6, 20% Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® GFT33N051-NBK2 Nylon 66, 33% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced GM 167A Black color matchAll information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-BKDX9 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® MRGF30/10 42H-GY1 Nylon 6, 30% Mineral and 10% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
Wellman Wellamid® MRGF30/10 42H-NBK1 Nylon 6, 30% Mineral and 10% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Time 86400 sec |
0.010 - 0.012 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.18 mm |
0.010 - 0.012 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |