Wellman Wellamid® MRGF30/10 42H-NBK1 Nylon 6, 30% Mineral and 10% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Wellman Wellamid® MRGF30/10 42H-NBK1 Nylon 6, 30% Mineral and 10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 145 MPa
21000 psi
ISO 178-93
Flexural Modulus 9.00 GPa
1310 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-93
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in